Cleansing Wipe Concentrate

Author Image

By: TOM BRANNA

Editor

Cleansing Wipe Concentrate
Ingredients
%

Phase A

  • Deionized water
  • 57.69
  • Glycerin
  • 8.00
  • Propylene glycol
  • 2.50
  • Dipropylene glycol
  • 1.50
  • Sodium lauroyl sarcosinate (30% active)
  • 13.33
  • Ammoniun lauryl sulfate (28% active)
  • 13.33
  • SoftCAT polymer SK-L (Polyquaternium-67)
  • 0.25

Phase B

  • Mineral oil
  • 2.00
  • Stearyl alcohol
  • 0.50
  • Cetyl alcohol
  • 0.50

Phase C

  • DMDM hydantoin
  • 0.40
  • Fragrance
  • q.s.

Procedure

Disperse the SoftCAT SK-L in rapidly agitating, room temperature water. Allow to disperse completely. Once the polymer is dispersed, heat the solution to 60-65˚C until clear. Add the  sodium lauroyl sarcosinate, ammoniun lauryl sulfate, glycerin, propylene glycol and dipropylene glycol to the polymer solution, one at a time, in order, waiting for uniformity before adding the next. Heat entire formulation to 60-65˚C. In a separate container, combine the ingredients of phase B. Heat the ingredients to 60-65˚C until the fatty alcohols are dissolved. At temperature, add the contents of phase B to Phase A with good agitation. Mix thoroughly while cooling at 45˚C. Add the DMDM hydantoin and fragrance. Impregnate cloths with concentrate as desired.

More Information